Bixinta ODM China Magnet Bar&Ball Dhismaha Qaybaha Dhismayaasha 436PCS
Waxaan ku adkeysaneynaa mabda'a ah "tayada in lagu bilaabo, adeegga bilowga, horumar joogto ah iyo hal-abuurnimo si loola kulmo macaamiisha" maamulkaaga iyo "Ciladaha eber, cabashooyinka eber" sida ujeedada caadiga ah. Si aad u cajiib ah adeegeena, waxaan ku siin alaabta isticmaalaya tayada aadka u wanaagsan ee qiimaha macquulka ah ee Supply ODM China Magnet Bar & Ball Dhismaha Qaybaha Blocks 436PCS, Waxaan nahay mid ka mid ah 100% soo saarayaasha ugu weyn ee Shiinaha. Dhowr shirkadood oo ganacsi oo waaweyn ayaa alaabta naga soo dejisa, markaa waxaanu ku siin doonaa qiimaha ugu waxtarka badan ee tayada leh haddii aad danaynayso annaga.
Waxaan ku adkeysaneynaa mabda'a ah "tayada in lagu bilaabo, adeegga bilowga, horumar joogto ah iyo hal-abuurnimo si loola kulmo macaamiisha" maamulkaaga iyo "Ciladaha eber, cabashooyinka eber" sida ujeedada caadiga ah. Si aan u wacno adeegeena, waxaan bixinaa alaabooyinka anagoo adeegsanayna tayada aadka u wanaagsan ee qiimaha macquulka ahShiinaha Waxbarasho Toys iyo Magnetic Blocks qiimaha , U hoggaansanaanta mabda'a "Ka-ganacsiga iyo Run-raadinta, Saxnaanta iyo Midnimada", oo leh tikniyoolajiyadda asaasiga ah, shirkadeena waxay sii waddaa in ay soo saarto, oo u heellan inay ku siiso alaabada ugu qaalisan ee waxtarka leh iyo adeegga iibka ka dib. Waxaan si adag u aaminsanahay taas: Waxaan nahay kuwo aad u wanaagsan maadaama aan nahay kuwo takhasus leh.
Hordhac:
AlNiCo waxay asal ahaan ka kooban yihiin aluminium, nikkel, cobalt, copper, iron iyo titanium. Fasalada qaarkood cobalt iyo/ama titanium waa laga saari karaa. Sidoo kale alwaaxyadaan waxaa ku jiri kara waxyaabo lagu daro silikoon, columbium, zirconium ama walxo kale kuwaas oo kor u qaadaya jawaabta daaweynta kulaylka ee mid ka mid ah sifooyinka magnetic. AlNiCo Alloys waxaa lagu sameeyay habsocodyada birta ah ee shubka ama budada ah.
Tilmaam:
1. AlNiCo magnet waxa uu leeyahay soo-jiidhaynta sare ee hadhaaga laakiin ku khasbid hoose. Waxay u shaqeysaa si deggan heer kul aad u daran, iyadoo ilaalinaysa sifooyinkeeda magnetic inta u dhaxaysa -250ºC iyo 550ºC. Iyada oo ku saleysan kicinta birlabeedka sare, waxaa inta badan loo adeegsadaa cabbiraadda qalabka iyo nidaamyada ogaanshaha.
2. Alnico waa walxo jilicsan waxaana la bedeli karaa oo kaliya inta lagu jiro habka shubista. Hanuuninta waxa ka mid ah oo lagu gaadhay inta lagu jiro daawaynta kulaylka, soo saarista beer magnetic la jihada magnetization qeexan.
3. Awoodda qasabka ah ee hooseeya awgeed, AlNiCo magnets si fudud ayay u saamayn kartaa xoog birlabeedka rogan iyo saamaynta birta. Taasi waa sababta ay si fudud u dhimi karaan saamaynta dibadda. Sababtan awgeed, magnets-ka AlNiCo waa in aan la kaydin oo lagu shubaa tiirar isku mid ah oo iska soo horjeeda.
4. Wareegga furan, saamiga dhererka / dhexroorka (L/D) waa inuu ahaadaa ugu yaraan 4: 1. Dherer gaaban oo gaaban,
5. AlNiCo magnets waxay si fiican ugu dhaqmaan oksaydhka. Looma baahna daahan ilaalinta dusha sare.
Codsiyada:
Isticmaal alaabada xasaasiga ah sida Qalabka, Mitirka, Taleefannada Gacanta, Qaybaha Baabuurta, Aaladaha Electroacoustic, Matoorada, Waxbarashada iyo Aerospace Military, iwm.
Dhammaan qiimayaasha la sheegay waxaa lagu go'aamiyay iyadoo la adeegsanayo muunado caadi ah iyadoo loo eegayo IEC 60404-5. Tilmaamaha soo socdaa waxay u adeegaan sida qiyamka tixraaca oo way kala duwanaan karaan.
Cast AlNiCo Magnet Qalabka Jirka | ||||||||
Qalab | Darajo | Joogista | Rev. Temp.-Coeff. Ee Br | Qasab | Rev. Temp.-Coeff. ee Hcj | Max. Alaabta Tamarta | Max. Heerkulka shaqada | Cufnaanta |
Br (KGs) | Hcb (Adiga) | (BH) ugu badnaan. (MGOe) | g/cm³ | |||||
Istropic | LN9 | 6.8 | -0.03 | 0.38 | -0.02 | 1.13 | 450 ℃ | 6.9 |
Istropic | LN10 | 6.0 | -0.03 | 0.50 | -0.02 | 1.20 | 450 ℃ | 6.9 |
Istropic | LNG12 | 7.2 | -0.03 | 0.50 | +0.02 | 1.55 | 450 ℃ | 7.0 |
Istropic | LNG13 | 7.0 | -0.03 | 0.60 | +0.02 | 1.60 | 450 ℃ | 7.0 |
Istropic | LNGT18 | 5.8 | -0.025 | 1.25 | +0.02 | 2.20 | 550 ℃ | 7.3 |
Anisotropic | LNG37 | 12.0 | -0.02 | 0.60 | +0.02 | 1.65 | 525℃ | 7.3 |
Anisotropic | LNG40 | 12.5 | -0.02 | 0.60 | +0.02 | 5.00 | 525℃ | 7.3 |
Anisotropic | LNG44 | 12.5 | -0.02 | 0.65 | +0.02 | 5.50 | 525℃ | 7.3 |
Anisotropic | LNG52 | 13.0 | -0.02 | 0.70 | +0.02 | 6.50 | 525℃ | 7.3 |
Anisotropic | LNG60 | 13.5 | -0.02 | 0.74 | +0.02 | 7.50 | 525℃ | 7.3 |
Anisotropic | LNGT28 | 10.8 | -0.02 | 0.72 | +0.03 | 3.50 | 525℃ | 7.3 |
Anisotropic | LNGT36J | 7.0 | -0.025 | 1.75 | +0.02 | 4.50 | 550 ℃ | 7.3 |
Anisotropic | LNGT32 | 8.0 | -0.025 | 1.25 | +0.02 | 4.00 | 550 ℃ | 7.3 |
Anisotropic | LNGT40 | 8.0 | -0.025 | 1.38 | +0.02 | 5.00 | 550 ℃ | 7.3 |
Anisotropic | LNGT60 | 9.0 | -0.025 | 1.38 | +0.02 | 7.50 | 550 ℃ | 7.3 |
Anisotropic | LNGT72 | 10.5 | -0.025 | 1.40 | +0.02 | 9.00 | 550 ℃ | 7.3 |
Guryaha Jirka ee AlNiCo Magnet ee Sintered | |||||||||
Qalab | Darajo | Joogista | Rev. Temp.-Coeff. Ee Br | Qasab | Qasab | Rev. Temp.-Coeff. ee Hcj | Max. Alaabta Tamarta | Max. Heerkulka shaqada | Cufnaanta |
Br (KGs) | Hcb (KA/m) | Hcj (KA/m) | (BH) ugu badnaan (KJ/m³) | g/cm³ | |||||
Istropic | SALNICO4/1 | 8.7-8.9 | -0.02 | 9-11 | 10-12 | -0.03-0.03 | 3.2-4.8 | 750 ℃ | 6.8 |
Istropic | SALNICO8/5 | 5.3-6.2 | -0.02 | 45-50 | 47-52 | -0.03-0.03 | 8.5-9.5 | 750 ℃ | 6.8 |
Istropic | SALNICO10/5 | 6.3-7.0 | -0.02 | 48-56 | 50-58 | -0.03-0.03 | 9.5-11.0 | 780℃ | 6.8 |
Istropic | SALNICO12/5 | 7.0-7.5 | -0.02 | 50-56 | 53-58 | -0.03-0.03 | 11.0-13.0 | 800 ℃ | 7 |
Istropic | SALNICO14/5 | 7.3-8.0 | -0.02 | 47-50 | 50-53 | -0.03-0.03 | 13.0-15.0 | 790℃ | 7.1 |
Istropic | SALNICO 14/6 | 6.2-8.1 | -0.02 | 56-64 | 58-66 | -0.03-0.03 | 14.0-16.0 | 790℃ | 7.1 |
Istropic | SALNICO14/8 | 5.5-6.1 | -0.01 | 75-88 | 80-92 | -0.03-0.03 | 14.0-16.0 | 850 ℃ | 7.1 |
Istropic | SALNICO18/10 | 5.7-6.2 | -0.01 | 92-100 | 99-107 | -0.03-0.03 | 16.0-19.0 | 860℃ | 7.2 |
Anisotropic | SALNICO35/5 | 11-12 | -0.02 | 48-52 | 50-54 | -0.03-0.03 | 35.0-39.0 | 850 ℃ | 7.2 |
Anisotropic | SALNICO29/6 | 9.7-10.9 | -0.02 | 58-64 | 60-66 | -0.03-0.03 | 29.0-33.0 | 860℃ | 7.2 |
Anisotropic | SALNICO32/10 | 7.7-8.7 | -0.01 | 90-104 | 94-109 | -0.03-0.03 | 33.0-38.0 | 860℃ | 7.2 |
Anisotropic | SALNICO33/11 | 7.0-8.0 | -0.01 | 107-115 | 111-119 | -0.03-0.03 | 33.0-38.0 | 860℃ | 7.2 |
Anisotropic | SALNICO39/12 | 8.3-9.0 | -0.01 | 115-123 | 119-127 | -0.03-0.03 | 39.0-43.0 | 860℃ | 7.25 |
Anisotropic | SALNICO44/12 | 9.0-9.5 | -0.01 | 119-127 | 124-132 | -0.03-0.03 | 44.0-48.0 | 860℃ | 7.25 |
Anisotropic | SALNICO37/15 | 7.0-8.0 | -0.1 | 143-151 | 150-158 | -0.03-0.03 | 37.0-41.0 | 870℃ | 7.2 |
Fiiro gaar ah:
Waxaan ahaanaynaa sidii kor ku xusan ilaa macmiilku caddeeyo. Heerkulka Curie iyo isku xidhka heerkulku waa tixraac kaliya, ma aha aasaaska go'aanka.
Heerkulka shaqada ugu badan ee magnet waa la bedeli karaa iyadoo ay ugu wacan tahay saamiga dhererka iyo dhexroorka iyo arrimaha deegaanka.