Shiinaha Qiimaha jaban ee Shiinaha N48 Macmiil xoog leh Magnetic Ainico NdFeB Magnet leh Assembly&Drig
Waxaan diyaar u ahayn inaan wadaagno aqoontayada suuq-geynta intarneedka adduunka oo dhan waxaanan kugula talineynaa baayacmushtar ku habboon heerarka ugu daran. Marka Qalabka Profi wuxuu kuu soo bandhigayaa qiimaha ugu fiican ee lacagta waxaanan diyaar u nahay inaan isku horumarino midba midka kale Shiinaha Qiimo jaban Shiinaha N48 Macaamiisha Strong Magnetic Ainico NdFeB Magnet oo leh Golaha & Dheriga, Shaybaarkayaga hadda waa "National Lab of Diesel engine Turbo technology" , and we Lahaanshaha shaqaale R&D u qalma iyo xarun imtixaan oo dhamaystiran.
Waxaan diyaar u ahayn inaan wadaagno aqoontayada suuq-geynta intarneedka adduunka oo dhan waxaanan kugula talineynaa baayacmushtar ku habboon heerarka ugu daran. Markaa Profi Tools waxay kuu soo bandhigaysaa qiimaha lacageed ee ugu wanaagsan waxaanan diyaar u nahay inaan is garabsano midba midka kaleChina Pot Magnet,Magnet Joogta ah , Waxaan si sii kordheysa u ballaarineynaa saamigayaga suuqa caalamiga ah oo ku saleysan alaab tayo leh iyo xalal, adeeg aad u fiican, qiimo macquul ah iyo bixinta waqtigeeda. Xusuusnow inaad nala soo xidhiidho wakhti kasta wixii macluumaad dheeraad ah.
Hordhac:
AlNiCo waxay asal ahaan ka kooban yihiin aluminium, nikkel, cobalt, copper, iron iyo titanium. Fasalada qaarkood cobalt iyo/ama titanium waa laga saari karaa. Sidoo kale alwaaxyadaan waxaa ku jiri kara waxyaabo lagu daro silikoon, columbium, zirconium ama walxo kale kuwaas oo kor u qaadaya jawaabta daaweynta kulaylka ee mid ka mid ah sifooyinka magnetic. AlNiCo Alloys waxaa lagu sameeyay habsocodyada birta ah ee shubka ama budada ah.
Tilmaam:
1. AlNiCo magnet waxay leedahay soo-jiidhaynta sare ee soo-jiidashada laakiin qasabku wuu hooseeyaa. Waxay u shaqeysaa si deggan heer kul aad u daran, iyadoo ilaalinaysa sifooyinkeeda magnetic inta u dhaxaysa -250ºC iyo 550ºC. Iyada oo ku saleysan kicinta birlabeedka sare, waxaa inta badan loo adeegsadaa cabbiraadda qalabka iyo nidaamyada ogaanshaha.
2. Alnico waa walxo jilicsan waxaana la bedeli karaa oo kaliya inta lagu jiro habka shubista. Hanuuninta waxaa ka mid ah oo lagu gaaray inta lagu guda jiro daaweynta kulaylka, soo saarista beer magnetic la jihada magnetization qeexan.
3. Awoodda qasabka ah ee hooseeya awgeed, AlNiCo magnets si fudud ayay u saamayn kartaa xoog birlabeedka rogan iyo saamaynta birta. Taasi waa sababta ay si fudud u dhimi karaan saamaynta dibadda. Sababtan awgeed, magnets-ka AlNiCo waa in aan la kaydin oo lagu shubaa tiirar isku mid ah oo iska soo horjeeda.
4. Wareegga furan, saamiga dhererka / dhexroorka (L/D) waa inuu ahaadaa ugu yaraan 4: 1. Dherer gaaban oo gaaban,
5. AlNiCo magnets waxay si fiican ugu dhaqmaan oksaydhka. Looma baahna daahan ilaalinta dusha sare.
Codsiyada:
Isticmaal alaabada xasaasiga ah sida Qalabka, Mitirka, Taleefannada Gacanta, Qaybaha Baabuurta, Aaladaha Electroacoustic, Matoorada, Waxbarashada iyo Aerospace Military, iwm.
Dhammaan qiimayaasha la sheegay waxaa lagu go'aamiyay iyadoo la adeegsanayo muunado caadi ah iyadoo loo eegayo IEC 60404-5. Tilmaamaha soo socdaa waxay u adeegaan sida qiyamka tixraaca waana kala duwanaan karaan.
Cast AlNiCo Magnet Qalabka Jirka | ||||||||
Qalab | Darajo | Joogista | Rev. Temp.-Coeff. Ee Br | Qasab | Rev. Temp.-Coeff. ee Hcj | Max. Alaabta Tamarta | Max. Heerkulka shaqada | Cufnaanta |
Br (KGs) | Hcb (Adiga) | (BH) ugu badnaan. (MGOe) | g/cm³ | |||||
Istropic | LN9 | 6.8 | -0.03 | 0.38 | -0.02 | 1.13 | 450 ℃ | 6.9 |
Istropic | LN10 | 6.0 | -0.03 | 0.50 | -0.02 | 1.20 | 450 ℃ | 6.9 |
Istropic | LNG12 | 7.2 | -0.03 | 0.50 | +0.02 | 1.55 | 450 ℃ | 7.0 |
Istropic | LNG13 | 7.0 | -0.03 | 0.60 | +0.02 | 1.60 | 450 ℃ | 7.0 |
Istropic | LNGT18 | 5.8 | -0.025 | 1.25 | +0.02 | 2.20 | 550 ℃ | 7.3 |
Anisotropic | LNG37 | 12.0 | -0.02 | 0.60 | +0.02 | 1.65 | 525℃ | 7.3 |
Anisotropic | LNG40 | 12.5 | -0.02 | 0.60 | +0.02 | 5.00 | 525℃ | 7.3 |
Anisotropic | LNG44 | 12.5 | -0.02 | 0.65 | +0.02 | 5.50 | 525℃ | 7.3 |
Anisotropic | LNG52 | 13.0 | -0.02 | 0.70 | +0.02 | 6.50 | 525℃ | 7.3 |
Anisotropic | LNG60 | 13.5 | -0.02 | 0.74 | +0.02 | 7.50 | 525℃ | 7.3 |
Anisotropic | LNGT28 | 10.8 | -0.02 | 0.72 | +0.03 | 3.50 | 525℃ | 7.3 |
Anisotropic | LNGT36J | 7.0 | -0.025 | 1.75 | +0.02 | 4.50 | 550 ℃ | 7.3 |
Anisotropic | LNGT32 | 8.0 | -0.025 | 1.25 | +0.02 | 4.00 | 550 ℃ | 7.3 |
Anisotropic | LNGT40 | 8.0 | -0.025 | 1.38 | +0.02 | 5.00 | 550 ℃ | 7.3 |
Anisotropic | LNGT60 | 9.0 | -0.025 | 1.38 | +0.02 | 7.50 | 550 ℃ | 7.3 |
Anisotropic | LNGT72 | 10.5 | -0.025 | 1.40 | +0.02 | 9.00 | 550 ℃ | 7.3 |
Guryaha Jirka ee AlNiCo Magnet ee Sintered | |||||||||
Qalab | Darajo | Joogista | Rev. Temp.-Coeff. Ee Br | Qasab | Qasab | Rev. Temp.-Coeff. ee Hcj | Max. Alaabta Tamarta | Max. Heerkulka shaqada | Cufnaanta |
Br (KGs) | Hcb (KA/m) | Hcj (KA/m) | (BH) ugu badnaan (KJ/m³) | g/cm³ | |||||
Istropic | SALNICO4/1 | 8.7-8.9 | -0.02 | 9-11 | 10-12 | -0.03-0.03 | 3.2-4.8 | 750 ℃ | 6.8 |
Istropic | SALNICO8/5 | 5.3-6.2 | -0.02 | 45-50 | 47-52 | -0.03-0.03 | 8.5-9.5 | 750 ℃ | 6.8 |
Istropic | SALNICO10/5 | 6.3-7.0 | -0.02 | 48-56 | 50-58 | -0.03-0.03 | 9.5-11.0 | 780℃ | 6.8 |
Istropic | SALNICO12/5 | 7.0-7.5 | -0.02 | 50-56 | 53-58 | -0.03-0.03 | 11.0-13.0 | 800 ℃ | 7 |
Istropic | SALNICO14/5 | 7.3-8.0 | -0.02 | 47-50 | 50-53 | -0.03-0.03 | 13.0-15.0 | 790℃ | 7.1 |
Istropic | SALNICO 14/6 | 6.2-8.1 | -0.02 | 56-64 | 58-66 | -0.03-0.03 | 14.0-16.0 | 790℃ | 7.1 |
Istropic | SALNICO14/8 | 5.5-6.1 | -0.01 | 75-88 | 80-92 | -0.03-0.03 | 14.0-16.0 | 850 ℃ | 7.1 |
Istropic | SALNICO18/10 | 5.7-6.2 | -0.01 | 92-100 | 99-107 | -0.03-0.03 | 16.0-19.0 | 860℃ | 7.2 |
Anisotropic | SALNICO35/5 | 11-12 | -0.02 | 48-52 | 50-54 | -0.03-0.03 | 35.0-39.0 | 850 ℃ | 7.2 |
Anisotropic | SALNICO29/6 | 9.7-10.9 | -0.02 | 58-64 | 60-66 | -0.03-0.03 | 29.0-33.0 | 860℃ | 7.2 |
Anisotropic | SALNICO32/10 | 7.7-8.7 | -0.01 | 90-104 | 94-109 | -0.03-0.03 | 33.0-38.0 | 860℃ | 7.2 |
Anisotropic | SALNICO33/11 | 7.0-8.0 | -0.01 | 107-115 | 111-119 | -0.03-0.03 | 33.0-38.0 | 860℃ | 7.2 |
Anisotropic | SALNICO39/12 | 8.3-9.0 | -0.01 | 115-123 | 119-127 | -0.03-0.03 | 39.0-43.0 | 860℃ | 7.25 |
Anisotropic | SALNICO44/12 | 9.0-9.5 | -0.01 | 119-127 | 124-132 | -0.03-0.03 | 44.0-48.0 | 860℃ | 7.25 |
Anisotropic | SALNICO37/15 | 7.0-8.0 | -0.1 | 143-151 | 150-158 | -0.03-0.03 | 37.0-41.0 | 870℃ | 7.2 |
Fiiro gaar ah:
Waxaan ahaanaynaa sidii kor ku xusan ilaa macmiilku caddeeyo. Heerkulka Curie iyo isku xidhka heerkulku waa tixraac kaliya, ma aha aasaaska go'aanka.
Heerkulka shaqada ugu badan ee magnet waa la bedeli karaa iyadoo ay ugu wacan tahay saamiga dhererka iyo dhexroorka iyo arrimaha deegaanka.