Warshada China ugu raqiisan Magnets dhoobada adag ee Ferrite Magnet Iibiyaha Gaarka ah Ceramic Ferrite Magnet
Waxaan dooneynaa inaan aragno tayada tayada leh ee abuurista oo aan siino taageerada ugu habboon iibsadayaasha gudaha iyo dibaddaFerriteMagnetsFerrite Alaab-qeybiyaha Magnet Custom Ceramic Ferrite Magnets, Marna ma joojineyno hagaajinta farsamadayada iyo tayada sare si aan uga caawino sii wadida isticmaalka isbedelka warshadahan oo aan ula kulano ku qanacsanaantaada si wax ku ool ah. Haddii ay dhacdo in aad xiiso u qabto alaabtayada, fadlan si xor ah noogu soo wac.
Waxaan rabnaa in aan aragno tayada xun ee abuurista oo aan siino taageerada ugu habboon ee iibsada gudaha iyo dibaddaba si kal iyo laab ahShiinaha Ferrite Magnet,Ferrite Marka ay soo saarto, iyada oo u adeegsanaysa habka ugu weyn ee adduunka ee loogu talagalay hawlgal la isku halleyn karo, qiimo jaban, oo ku habboon doorashada dukaamaysiga Jeddah. Shirkadeena. Waxay ku taal gudaha magaalooyinka ilbaxnimada qaranka, gaadiidka mareegaha waa mid aan dhib lahayn, juquraafi ahaan iyo duruufo dhaqaale oo gaar ah. Waxaan raacnaa "dadka ku jihaysan, wax soo saarka si taxadar leh, maskaxiyan, samayno falsafada shirkadda". Maareyn tayo wanaagsan oo adag, adeeg fantastik ah, kharash la awoodi karo oo Jeddah ah ayaa ah meesha aan ka taaganahay goobta tartamayaasha. Haddii loo baahdo, ku soo dhawoow inaad nagala soo xidhiidho boggayaga internetka ama la talinta telefoonka, waxaanu ku farxi doonaa inaanu ku adeegno.
Hordhac:
Magnets SmCo waxay matalaan jiilkii ugu dambeeyay ee agabka birlabeedka. Waxa la sameeyay in ka badan 40 sano ka hor waxayna soo bandhigeen waagii matoorada magnetka joogtada ah. Waqtigaas, birahan dhulka dhifka ah aad bay qaali u ahaayeen. Intii lagu jiray sannadihii 1980-aadkii, agabka SmCo waxa si isa soo taraysa loogu beddelay magnets NdFeB. Sababo la xiriira kor u kaca qiimaha laxaadka leh ee dhulka naadirka ah ee neodymium iyo dysprosium (Nd/Dy), maaddadani hadda waxay dib u heshay caannimadeeda codsiyada heerkul sare (150°C – 200°C). Si kastaba ha ahaatee, waxaa jira xad loo dejiyay walxaha marka la eego sii joogida ugu badan. Laba nooc oo waaweyn oo magnets SmCo ah ayaa diyaar ah, 1: 5 nooca (SmCo5) iyo 2:17 nooca (Sm2Co17). Magnets-yada SmCo waxay leeyihiin sifooyin magnetic heer sare ah iyo sifooyin heerkul sare ah.
Faa'iidada:
Isticmaalka birlabyadaan waxaa lagu shardiyaa heerkulka kala duwan ee ka socda 250ºC ilaa 350ºC heerkulkooda Curie wuxuu noqon karaa ilaa 710 ilaa 880 °C. Sidaa darteed, magnet SmCo waxay leedahay xasiloonida magnetka ugu fiican sababtoo ah caabbinta sare ee heerkulka sare. Magnets SmCo waxaa lagu gartaa iska caabin daxalka aad u sarreeya, ma daahan loo baahan yahay ilaalinta dusha.
Tilmaam:
Khasaarada birta SmCo ayaa ah jajabnaanta calaamadsan ee walxaha - arrin ay tahay in si gaar ah loo tixgeliyo inta lagu jiro habaynta. Magnet-ka waxa lagu galvanized ama lagu dahaadhay by cathodic electrodeposition codsiyada qaarkood.
Codsiga:
Meelaha heerkulka sare ee hawlgalka, daxalka sare iyo caabbinta oksaydhisku waa muhiim. Sida elektaroonigga magnetron, gudbinta magnetic, daawaynta Magnetic, Magnistor, iwm.
Dhammaan qiimayaasha la sheegay waxaa lagu go'aamiyay iyadoo la adeegsanayo muunado caadi ah iyadoo loo eegayo IEC 60404-5. Tilmaamaha soo socdaa waxay u adeegaan sida qiyamka tixraaca waana kala duwanaan karaan. ugu badnaan heerkulka shaqayntu waa
ku xiran cabbirka magnetka iyo codsiga gaarka ah. Wixii macluumaad dheeraad ah fadlan
la xidhiidh injineeradayada codsiga.
Guryaha Jirka ee Sintered SmCo Magnet | |||||||||
Qalab | Darajo | Joogista | Rev. Temp.- Coeff. Ee Br | Xoog ku Qasab ah | Xoogaga qasabka ah ee gudaha | Rev. Temp.-Coeff. ee Hcj | Max. Alaabta Tamarta | Max. Heerkulka shaqada | Cufnaanta |
Br (KGs) | Hcb (Adiga) | Hcj (Adiga) | (BH) ugu badnaan. (MGOe) | g/cm³ | |||||
SmCo5 | XG16 | 8.1-8.5 | -0.050 | 7.8-8.3 | 15-23 | -0.30 | 14-16 | 250 ℃ | 8.3 |
XG18 | 8.5-9.0 | -0.050 | 8.3-8.8 | 15-23 | -0.30 | 16-18 | 250 ℃ | 8.3 | |
XG20 | 9.0-9.4 | -0.050 | 8.5-9.1 | 15-23 | -0.30 | 19-21 | 250 ℃ | 8.3 | |
XG22 | 9.2-9.6 | -0.050 | 8.9-9.4 | 15-23 | -0.30 | 20-22 | 250 ℃ | 8.3 | |
XG24 | 9.6-10.0 | -0.050 | 9.2-9.7 | 15-23 | -0.30 | 22-24 | 250 ℃ | 8.3 | |
XG16S | 7.9-8.4 | -0.050 | 7.7-8.3 | ≥23 | -0.28 | 15-17 | 250 ℃ | 8.3 | |
XG18S | 8.4-8.9 | -0.050 | 8.1-8.7 | ≥23 | -0.28 | 17-19 | 250 ℃ | 8.3 | |
XG20S | 8.9-9.3 | -0.050 | 8.6-9.2 | ≥23 | -0.28 | 19-21 | 250 ℃ | 8.3 | |
XG22S | 9.2-9.6 | -0.050 | 8.9-9.5 | ≥23 | -0.28 | 21-23 | 250 ℃ | 8.3 | |
XG24S | 9.6-10.0 | -0.050 | 9.3-9.9 | ≥23 | -0.28 | 23-25 | 250 ℃ | 8.3 | |
Sm2Co17 | XG24H | 9.5-10.2 | -0.025 | 8.7-9.6 | ≥25 | -0.20 | 22-24 | 350 ℃ | 8.3 |
XG26H | 10.2-10.5 | -0.030 | 9.4-10.0 | ≥25 | -0.20 | 24-26 | 350 ℃ | 8.3 | |
XG28H | 10.3-10.8 | -0.035 | 9.5-10.2 | ≥25 | -0.20 | 26-28 | 350 ℃ | 8.3 | |
XG30H | 10.8-11.0 | -0.035 | 9.9-10.5 | ≥25 | -0.20 | 28-30 | 350 ℃ | 8.3 | |
XG32H | 11.0-11.3 | -0.035 | 10.2-10.8 | ≥25 | -0.20 | 29-32 | 350 ℃ | 8.3 | |
XG22 | 9.3-9.7 | -0.020 | 8.5-9.3 | ≥18 | -0.20 | 20-23 | 300 ℃ | 8.3 | |
XG24 | 9.5-10.2 | -0.025 | 8.7-9.6 | ≥18 | -0.20 | 22-24 | 300 ℃ | 8.3 | |
XG26 | 10.2-10.5 | -0.030 | 9.4-10.0 | ≥18 | -0.20 | 24-26 | 300 ℃ | 8.3 | |
XG28 | 10.3-10.8 | -0.035 | 9.5-10.2 | ≥18 | -0.20 | 26-28 | 300 ℃ | 8.3 | |
XG30 | 10.8-11.0 | -0.035 | 9.9-10.5 | ≥18 | -0.20 | 28-30 | 300 ℃ | 8.3 | |
XG32 | 11.0-11.3 | -0.035 | 10.2-10.8 | ≥18 | -0.20 | 29-32 | 300 ℃ | 8.3 | |
XG26M | 10.2-10.5 | -0.035 | 8.5-9.8 | 12-18 | -0.20 | 24-26 | 300 ℃ | 8.3 | |
XG28M | 10.3-10.8 | -0.035 | 8.5-10.0 | 12-18 | -0.20 | 26-28 | 300 ℃ | 8.3 | |
XG30M | 10.8-11.0 | -0.035 | 8.5-10.5 | 12-18 | -0.20 | 28-30 | 300 ℃ | 8.3 | |
XG32M | 11.0-11.3 | -0.035 | 8.5-10.7 | 12-18 | -0.20 | 29-32 | 300 ℃ | 8.3 | |
XG24L | 9.5-10.2 | -0.025 | 6.8-9.0 | 8-12 | -0.20 | 22-24 | 250 ℃ | 8.3 | |
XG26L | 10.2-10.5 | -0.035 | 6.8-9.4 | 8-12 | -0.20 | 24-26 | 250 ℃ | 8.3 | |
XG28L | 10.3-10.8 | -0.035 | 6.8-9.6 | 8-12 | -0.20 | 26-28 | 250 ℃ | 8.3 | |
XG30L | 10.8-11.5 | -0.035 | 6.8-10.0 | 8-12 | -0.20 | 28-30 | 250 ℃ | 8.3 | |
XG32L | 11.0-11.5 | -0.035 | 6.8-10.2 | 8-12 | -0.20 | 29-32 | 250 ℃ | 8.3 | |
Fiiro gaar ah: |